Phosphorous Removal from Iron Ore with a Low Temperature ...
to the iron ore before the heat treatment, similar phosphorous removal was achieved with a heating temperature of 300 - 350C. It was considered that dehydroxylation of the goethite in the presence of the hydroxide makes the phosphorous available for removal with a water leach. As well, 50 per cent of