Cyanide-free gold leaching in exceptionally mild chloride ...
In test 9, the gold extraction was 78% but the presence of carbon increased it up to 94% (test 10). During ferric leaching (i.e., without added cupric ions and bromide), gold extraction was only 41% (test 11) whereas with CICl, the gold extraction increased up to 85% (test 12).