The Rise of Nickel Laterites and Advances in Sulphide ...
Sulphide Hydrometallurgy - CESL • Process − Comminution – 25 to 45 micron ... • Process − Ultrafine grinding − Pressure Oxidation Leach > Sulphuric acid > Pure oxygen > 10 bar ... − Isamill grinding − Oxidation leach > 1 bar > 70oC > Supersonic pure oxygen − CCDs, impurity removal, MHP ...